Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 PEI Static Dissipative Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Semitron® ESd 420 PEI Polyetherimide electro static dissipative shapes exhibit high strength and stiffness, and excellent resistivity in the 10E6 to 10E9 ohms per square range. This grade in particular excels in high temperature environments, making it ideal for extreme structural applications in semiconductor and electronics markets.

Key Words: formerly Semitron® ESd 420- CM
Available Properties
  • Specific Gravity
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Tensile Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Shear Strength
  • Charpy Impact, Notched
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Transition Temp, Tg
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  • Data Sheet Region
  • Targeted Usage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.