Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Water Absorption at Saturation 0.210 %0.210 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 106106ASTM D785
Tensile Strength 114 MPa16500 psiISO 527-1/-2 (7)
Elongation at Yield 4.00 %4.00 %ISO 527-1/-2 (7)
Compressive Yield Strength  45.0 MPa
@Strain 1.00 %
6530 psi
@Strain 1.00 %
ISO 604 (10)
 86.0 MPa
@Strain 2.00 %
12500 psi
@Strain 2.00 %
ISO 604 (10)
 144 MPa
@Strain 5.00 %
20900 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 83.0 MPa12000 psiASTM D732
Charpy Impact, Notched 0.320 J/cm²1.52 ft-lb/in²ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C25.0 µin/in-°FASTM E-831 (TMA)
 45.0 µm/m-°C
@Temperature 23.0 - 100 °C
25.0 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.249 W/m-K1.73 BTU-in/hr-ft²-°F
Melting Point 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 249 °C480 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.