Searches:   Step-by-Step Selector  | Quick Database Search

Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA FR PA66 Nylon 66, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: This flame-retardant nylon developed to fulfill UL94-V0 requirements for plastic flammability ratings. This nylon 66 is often used in transport and railway applications.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 87.087.0ASTM D785
Tensile Strength 79.0 MPa11500 psiISO 527-1/-2 (7)
Elongation at Yield 7.00 %7.00 %ISO 527-1/-2 (7)
Compressive Yield Strength  35.0 MPa
@Strain 1.00 %
5080 psi
@Strain 1.00 %
ISO 604 (10)
 65.0 MPa
@Strain 2.00 %
9430 psi
@Strain 2.00 %
ISO 604 (10)
 98.0 MPa
@Strain 5.00 %
14200 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.370 W/m-K2.57 BTU-in/hr-ft²-°F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak LimitedLimited
Alcohols LimitedLimited
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.