Material Notes: |
This PA66 grade exhibits an ideal balance of strength, toughness, and wear resistance. This versatile, high-performance nylon material offers broad size and shape availability and is commonly used for general purpose bearing and wear components.
|
Key Words: |
Extruded, UV Stabilized, Nylon 66 |