Mitsubishi Chemical Advanced Materials Semitron™ ESd 410C PEI Static Dissipative Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Semitron™ ESd 410C is an electrostatic dissipative PEI material that exhibits excellent dimensional stability characteristics and resistance to extreme temperatures, ideal for semiconductor and electronics handling.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Water Absorption at Saturation 1.10 %1.10 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 115115ASTM D785
Hardness, Shore D 85.085.0ISO 868
Tensile Strength 62.0 MPa8990 psiISO 527-1/-2 (7)
Flexural Strength 80.0 MPa11600 psiISO 178 (12)
Compressive Yield Strength  44.0 MPa
@Strain 1.00 %
6380 psi
@Strain 1.00 %
ISO 604 (10)
 76.0 MPa
@Strain 2.00 %
11000 psi
@Strain 2.00 %
ISO 604 (10)
 114 MPa
@Strain 5.00 %
16500 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 62.0 MPa8990 psiASTM D732
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 10000 ohm10000 ohmANSI/ESD STM 11.11
Dielectric Constant 3.00
@Frequency 1.00e+6 Hz
3.00
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.00130
@Frequency 1.00e+6 Hz
0.00130
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.4 µm/m-°C18.0 µin/in-°FASTM E-831 (TMA)
 40.0 µm/m-°C
@Temperature 23.0 - 100 °C
22.2 µin/in-°F
@Temperature 73.4 - 212 °F
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.2 µin/in-°F
@Temperature 73.4 - 302 °F
 45.0 µm/m-°C
@Temperature >=150 °C
25.0 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°F
 0.353 W/m-K2.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C338 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FASTM D648
Glass Transition Temp, Tg 210 °C410 °FDMA- Tan d
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic LimitedLimited
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Structural UsesStructural Uses
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.