Mitsubishi Chemical Advanced Materials Techtron™ 1000 PPS Extruded Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Unreinforced, Extruded

Material Notes: This PPS grade exhibits outstanding dimensional stability due to its minimal moisture absorption and low coefficient of linear thermal expansion, making the material easy to machine to close tolerances.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Water Absorption at Saturation 0.0300 %0.0300 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Hardness, Shore D 84.084.0ISO 868
Tensile Strength 102 MPa14800 psiISO 527-1/-2 (7)
Elongation at Yield 12.0 %12.0 %ISO 527-1/-2 (7)
Flexural Strength 155 MPa22500 psiISO 178 (12)
Compressive Yield Strength  39.0 MPa
@Strain 1.00 %
5660 psi
@Strain 1.00 %
ISO 604 (10)
 77.0 MPa
@Strain 2.00 %
11200 psi
@Strain 2.00 %
ISO 604 (10)
 122 MPa
@Strain 5.00 %
17700 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 62.0 MPa8990 psiASTM D732
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.00
@Frequency 1.00e+6 Hz
3.00
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1 (15)
 21.3 kV/mm540 kV/inASTM D149
Dissipation Factor 0.00130
@Frequency 1.00e+6 Hz
0.00130
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.4 µm/m-°C28.0 µin/in-°FASTM E-831 (TMA)
 60.0 µm/m-°C
@Temperature 23.0 - 100 °C
33.3 µin/in-°F
@Temperature 73.4 - 212 °F
 80.0 µm/m-°C
@Temperature 23.0 - 150 °C
44.4 µin/in-°F
@Temperature 73.4 - 302 °F
 145 µm/m-°C
@Temperature >=150 °C
80.6 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°F
 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Melting Point 282 °C540 °FASTM D3418
Maximum Service Temperature, Air 221 °C430 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Structural UsesStructural Uses
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.