Mitsubishi Chemical Advanced Materials Techtron™ GF40 PPS Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Techtron™ GF40 is a 40% glass fiber reinforced grade of PPS that exhibits higher stiffness and creep resistance than other PPS grades. Because of its improved dimensional stability, this grade excels in structural applications involving a high static load, even for long periods of time and at elevated temperatures.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 90.090.0ASTM D785
Tensile Strength 60.0 MPa8700 psiISO 527-1/-2 (7)
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear  45.0 µm/m-°C
@Temperature 23.0 - 100 °C
25.0 µin/in-°F
@Temperature 73.4 - 212 °F
 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
33.3 µin/in-°F
@Temperature 73.4 - 302 °F
 65.0 µm/m-°C
@Temperature >=150 °C
36.1 µin/in-°F
@Temperature >=302 °F
Melting Point 282 °C540 °FASTM D3418
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM905 / 291062