Searches:   Step-by-Step Selector  | Quick Database Search
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

<< Back to datasheet

Metric English
( This graph is merely a visual representation of the tabular data. It is not meant to predict any property behavior between data points.
Sample and/or test conditions are not necessarily identical for every data point; please note any comments beside any data points for details. )

Graph data in tabular format:
CTE, linearMetricEnglishComments
 55.8 µm/m-°C31.0 µin/in-°FASTM E-831 (TMA)
 55.0 µm/m-°C
@Temperature 23.0 - 100 °C
30.6 µin/in-°F
@Temperature 73.4 - 212 °F
 55.0 µm/m-°C
@Temperature 23.0 - 150 °C
30.6 µin/in-°F
@Temperature 73.4 - 302 °F
 70.0 µm/m-°C
@Temperature >=150 °C
38.9 µin/in-°F
@Temperature >=302 °F