Mitsubishi Chemical Advanced Materials Duratron™ D7015G PI Bearing Grade Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: This hot compression molded, 15% graphite filled PI is a bearing grade material with superior temperature and wear resistance, as well as a low coefficient of friction.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Water Absorption at Saturation 3.00 %3.00 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 115115ASTM D785
Hardness, Shore D 86.086.0ISO 868
Tensile Strength 105 MPa15200 psiISO 527-1/-2 (7)
Flexural Strength 150 MPa21800 psiISO 178 (12)
Compressive Yield Strength  40.0 MPa
@Strain 1.00 %
5800 psi
@Strain 1.00 %
ISO 604 (10)
 70.0 MPa
@Strain 2.00 %
10200 psi
@Strain 2.00 %
ISO 604 (10)
 130 MPa
@Strain 5.00 %
18900 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 90.0 MPa13100 psiASTM D732
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 10000 ohm10000 ohmANSI/ESD STM 11.11
Dielectric Strength 13.0 kV/mm330 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°FASTM E-831 (TMA)
 37.0 µm/m-°C
@Temperature 23.0 - 100 °C
20.6 µin/in-°F
@Temperature 73.4 - 212 °F
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.2 µin/in-°F
@Temperature 73.4 - 302 °F
 49.0 µm/m-°C
@Temperature >=150 °C
27.2 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.389 W/m-K2.70 BTU-in/hr-ft²-°F
 0.390 W/m-K2.71 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 299 °C570 °FContinuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air -196 °C-321 °F
 -196 °C-321 °F
Glass Transition Temp, Tg 391 °C735 °FDMA- Tan d
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic UnacceptableUnacceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Load + BearingLoad + Bearing
 
Descriptive Properties
ESd categoryConductive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.