Mitsubishi Chemical Advanced Materials Duratron™ D7000 PI Unfilled Polyimide
Categories:
Polymer
;
Thermoplastic
;
Polyimide, Thermoplastic
Material Notes:
This robust, compression molded PI offers outstanding electrical, thermal, and mechanical properties in high temperature applications, helping to extend service life and increase uptime.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Metric
English
Comments
Specific Gravity
1.40
g/cc
1.40
g/cc
ASTM D792
Water Absorption at Saturation
4.00 %
4.00 %
ASTM D570 (17)
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
120
120
ASTM D785
Tensile Strength
125
MPa
18100
psi
ISO 527-1/-2 (7)
Flexural Strength
180
MPa
26100
psi
ISO 178 (12)
Compressive Yield Strength
35.0
MPa
@Strain 1.00 %
5080
psi
@Strain 1.00 %
ISO 604 (10)
70.0
MPa
@Strain 2.00 %
10200
psi
@Strain 2.00 %
ISO 604 (10)
145
MPa
@Strain 5.00 %
21000
psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched
1.00
J/cm²
4.76
ft-lb/in²
ISO 179-1/1eA
Electrical Properties
Metric
English
Comments
Surface Resistivity per Square
1.00e+14
ohm
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
3.41
@Frequency 1.00e+6 Hz
3.41
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
27.6
kV/mm
700
kV/in
ASTM D149
37.0
kV/mm
940
kV/in
IEC 60243-1 (15)
Dissipation Factor
0.00380
@Frequency 1.00e+6 Hz
0.00380
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
72.0
µm/m-°C
40.0
µin/in-°F
ASTM E-831 (TMA)
40.0
µm/m-°C
@Temperature 23.0 - 100 °C
22.2
µin/in-°F
@Temperature 73.4 - 212 °F
42.0
µm/m-°C
@Temperature 23.0 - 150 °C
23.3
µin/in-°F
@Temperature 73.4 - 302 °F
52.0
µm/m-°C
@Temperature >=150 °C
28.9
µin/in-°F
@Temperature >=302 °F
Thermal Conductivity
0.220
W/m-K
1.53
BTU-in/hr-ft²-°F
0.220
W/m-K
1.53
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
299
°C
570
°F
Continuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air
-196
°C
-321
°F
-196
°C
-321
°F
Glass Transition Temp, Tg
374
°C
705
°F
DMA- Tan d
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Unacceptable
Unacceptable
Acids, Weak
Acceptable
Acceptable
Alcohols
Unacceptable
Unacceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Unacceptable
Alkalies, Weak
Unacceptable
Unacceptable
Chlorinated Solvents
Unacceptable
Unacceptable
Continuous Sunlight
Unacceptable
Unacceptable
Hot Water / Steam
Limited
Limited
Hydrocarbons - Aliphatic
Unacceptable
Unacceptable
Hydrocarbons - Aromatic
Unacceptable
Unacceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Unacceptable
Unacceptable
Miscellaneous Properties
Metric
English
Comments
Data Sheet Region
Americas
Americas
Targeted Usage
Structural Uses
Structural Uses
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
P1SM05s / 104384