Mitsubishi Chemical Advanced Materials Duratron™ D7000 PI Unfilled Polyimide
Categories:
Polymer
;
Thermoplastic
;
Polyimide, Thermoplastic
Material Notes:
This robust, compression molded PI offers outstanding electrical, thermal, and mechanical properties in high temperature applications, helping to extend service life and increase uptime.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.40
g/cc
ASTM D792
Water Absorption at Saturation
4.00 %
ASTM D570 (17)
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
120
ASTM D785
Tensile Strength
125
MPa
ISO 527-1/-2 (7)
Flexural Strength
180
MPa
ISO 178 (12)
Compressive Yield Strength
35.0
MPa
@Strain 1.00 %
ISO 604 (10)
70.0
MPa
@Strain 2.00 %
ISO 604 (10)
145
MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched
10.0
kJ/m²
ISO 179-1/1eA
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
3.41
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
37.0
kV/mm
IEC 60243-1 (15)
700
kV/in
ASTM D149
Dissipation Factor
0.00380
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Original Value
Comments
CTE, linear
40.0
µin/in-°F
ASTM E-831 (TMA)
40.0
µm/m-°C
@Temperature 23.0 - 100 °C
42.0
µm/m-°C
@Temperature 23.0 - 150 °C
52.0
µm/m-°C
@Temperature >=150 °C
Thermal Conductivity
0.220
W/m-K
1.53
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
570
°F
Continuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air
-321
°F
-196
°C
Glass Transition Temp, Tg
705
°F
DMA- Tan d
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Unacceptable
Acids, Weak
Acceptable
Alcohols
Unacceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Alkalies, Weak
Unacceptable
Chlorinated Solvents
Unacceptable
Continuous Sunlight
Unacceptable
Hot Water / Steam
Limited
Hydrocarbons - Aliphatic
Unacceptable
Hydrocarbons - Aromatic
Unacceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Unacceptable
Miscellaneous Properties
Original Value
Comments
Data Sheet Region
Americas
Targeted Usage
Structural Uses
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.