Mitsubishi Chemical Advanced Materials Nylatron™ 703 XL PA6 Cast, Wear Resistant, Zero 'Stick-Slip
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber/Solid Lube Filled

Material Notes: An ultra-high performance bearing grade PA6 with superior wear resistance and load bearing capabilities as well as a near zero level of stick-slip. Due to the elimination of stick-slip, an extraordinary amount of motion control for high-precision applications is gained.

Key Words: Polyamide
Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Water Absorption at Saturation 7.00 %7.00 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 59.059.0ASTM D785
Hardness, Shore D 73.073.0ISO 868
Tensile Strength 60.0 MPa8700 psiISO 527-1/-2 (7)
Elongation at Yield 6.00 %6.00 %ISO 527-1/-2 (7)
Compressive Yield Strength  26.0 MPa
@Strain 1.00 %
3770 psi
@Strain 1.00 %
ISO 604 (10)
 48.0 MPa
@Strain 2.00 %
6960 psi
@Strain 2.00 %
ISO 604 (10)
 69.0 MPa
@Strain 5.00 %
10000 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 88.2 µm/m-°C49.0 µin/in-°FASTM E-831 (TMA)
 85.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 140 °F
 100 µm/m-°C
@Temperature 23.0 - 100 °C
55.6 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Melting Point 216 °C420 °FASTM D3418
Maximum Service Temperature, Air 93.3 °C200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak LimitedLimited
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Load + BearingLoad + Bearing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM25M / 20114