Searches:   Step-by-Step Selector  | Quick Database Search

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron™ 703 XL PA6 Cast, Wear Resistant, Zero 'Stick-Slip
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber/Solid Lube Filled

Material Notes: An ultra-high performance bearing grade PA6 with superior wear resistance and load bearing capabilities as well as a near zero level of stick-slip. Due to the elimination of stick-slip, an extraordinary amount of motion control for high-precision applications is gained.

Key Words: Polyamide
Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Water Absorption at Saturation 7.00 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 59.0ASTM D785
Hardness, Shore D 73.0ISO 868
Tensile Strength 60.0 MPaISO 527-1/-2 (7)
Elongation at Yield 6.00 %ISO 527-1/-2 (7)
Compressive Yield Strength 26.0 MPa
@Strain 1.00 %
ISO 604 (10)
 48.0 MPa
@Strain 2.00 %
ISO 604 (10)
 69.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 49.0 µin/in-°FASTM E-831 (TMA)
 85.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 100 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.300 W/m-K
Melting Point 420 °FASTM D3418
Maximum Service Temperature, Air 200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 200 °FASTM D648
Minimum Service Temperature, Air -20.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Limited
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Miscellaneous PropertiesOriginal ValueComments
Data Sheet Region Americas
Targeted Usage Load + Bearing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM25M / 20114