Material Notes: |
Life Science Grade PSU stock shapes made from unfilled Udel™ PSU resin. Pre-assessed for biocompatibility on both resin and shape for up to 24 hours contact with body tissue according to USP VI and ISO 10993 and wetted contact in bioprocessing. Good hydrolysis resistance as well as great mechanical, thermal, and electrical properties.
|