Material Notes:

  • High impact resistance strength
  • Better resistance to cracking at low temperatures than Homopolymer Polypropylene
  • More pliable than homopolymer
  • Meets food handling guidelines
  • Chemical- and corrosion-resistant
  • No moisture absorption
  • FDA and 3-A Dairy CompliantAppropriate for applications to 180°F (82°C)
  • Resists most acids, alkalis and solvents
  • Meets FDA 21CFR 177.1520
  • Thermoforming performance
  • USDA, NSF and 3-A Dairy Complaint (natural color only)

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878ASTM D2240
Tensile Strength 33.1 MPa4800 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 12 %12 %ASTM D638
Tensile Modulus 1.19 GPa173 ksiASTM D638
Flexural Strength 33.1 MPa4800 psiASTM D790
Flexural Modulus 1.24 GPa180 ksiASTM D790
Compressive Strength 34.5 MPa5000 psi10% Def.; ASTM D695
Compressive Modulus 1.38 GPa200 ksiASTM D695
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.250.25Dry vs. Steel; QTM55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic UnacceptableUnacceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Miscellaneous PropertiesMetricEnglishComments
Targeted Usage Structural UsesStructural Uses
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.