Material Notes: |
- High impact resistance strength
- Better resistance to cracking at low temperatures than Homopolymer Polypropylene
- More pliable than homopolymer
- Meets food handling guidelines
- Chemical- and corrosion-resistant
- No moisture absorption
- FDA and 3-A Dairy CompliantAppropriate for applications to 180°F (82°C)
- Resists most acids, alkalis and solvents
- Meets FDA 21CFR 177.1520
- Thermoforming performance
- USDA, NSF and 3-A Dairy Complaint (natural color only)
Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials. |