Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 58.058.0ISO 868
Tensile Strength 19.0 MPa2760 psiISO 527-1/-2 (7)
Elongation at Yield 15.0 %15.0 %ISO 527-1/-2 (7)
Compressive Yield Strength  6.00 MPa
@Strain 1.00 %
870 psi
@Strain 1.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
1450 psi
@Strain 2.00 %
ISO 604 (10)
 16.0 MPa
@Strain 5.00 %
2320 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 10.0 J/cm²47.6 ft-lb/in²Partial Break; ISO 179-1/1eA
 13.0 J/cm²61.9 ft-lb/in²Double Notched
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 45.0 kV/mm1140 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 100 °C
111 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Minimum Service Temperature, Air -200 °C-328 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.