Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58.0ISO 868
Tensile Strength 19.0 MPaISO 527-1/-2 (7)
Elongation at Yield 15.0 %ISO 527-1/-2 (7)
Compressive Yield Strength 6.00 MPa
@Strain 1.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
ISO 604 (10)
 16.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 100 kJ/m²Partial Break; ISO 179-1/1eA
 130 kJ/m²Double Notched
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 45.0 kV/mmIEC 60243-1 (15)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.400 W/m-K
Minimum Service Temperature, Air -200 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.