Mitsubishi Chemical Advanced Materials TIVAR™ CleanStat™ EC FG UHMW-PE Electro Static Dissipative
Categories: Polymer; Thermoplastic; Polyethylene (PE); UHMW-PE

Material Notes: An electrically conductive UHMW-PE that meets both EU and FDA compliance requirements for food and pharmaceutical production and packaging. Easy to machine and leaves a cleaner work environment with less dust.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63.063.0ISO 868
Tensile Strength 20.0 MPa2900 psiISO 527-1/-2 (7)
Elongation at Yield 20.0 %20.0 %ISO 527-1/-2 (7)
Flexural Strength 18.0 MPa2610 psiISO 178 (12)
Compressive Yield Strength  6.00 MPa
@Strain 1.00 %
870 psi
@Strain 1.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
1450 psi
@Strain 2.00 %
ISO 604 (10)
 17.0 MPa
@Strain 5.00 %
2470 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 9.00 J/cm²42.8 ft-lb/in²Partial Break; ISO 179-1/1eA
 12.5 J/cm²59.5 ft-lb/in²Double Notched
 
Thermal PropertiesMetricEnglishComments
CTE, linear 300 µm/m-°C
@Temperature 23.0 - 100 °C
167 µin/in-°F
@Temperature 73.4 - 212 °F
Minimum Service Temperature, Air -150 °C-238 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Targeted Usage Load + BearingLoad + Bearing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.