Mitsubishi Chemical Advanced Materials TIVAR™ CleanStat™ EC FG UHMW-PE Electro Static Dissipative
Categories: Polymer; Thermoplastic; Polyethylene (PE); UHMW-PE

Material Notes: An electrically conductive UHMW-PE that meets both EU and FDA compliance requirements for food and pharmaceutical production and packaging. Easy to machine and leaves a cleaner work environment with less dust.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63.0ISO 868
Tensile Strength 20.0 MPaISO 527-1/-2 (7)
Elongation at Yield 20.0 %ISO 527-1/-2 (7)
Flexural Strength 18.0 MPaISO 178 (12)
Compressive Yield Strength 6.00 MPa
@Strain 1.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
ISO 604 (10)
 17.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 90.0 kJ/m²Partial Break; ISO 179-1/1eA
 125 kJ/m²Double Notched
 
Thermal PropertiesOriginal ValueComments
CTE, linear 300 µm/m-°C
@Temperature 23.0 - 100 °C
Minimum Service Temperature, Air -150 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Acceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Miscellaneous PropertiesOriginal ValueComments
Targeted Usage Load + Bearing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.