Mitsubishi Chemical Advanced Materials TIVAR™ VMX FG UHMW-PE Food Grade Ultra High Molecular Weight Polyethylene
Material Notes: A metal-detectable, food-grade polyethylene specifically developed to serve as a wear- and abrasion-resistant material with easy traceability in the food processing and packaging industries.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62.062.0ISO 868
Tensile Strength 20.0 MPa2900 psiISO 527-1/-2 (7)
Elongation at Yield 16.0 %16.0 %ISO 527-1/-2 (7)
Flexural Strength 20.0 MPa2900 psiISO 178 (12)
Compressive Yield Strength  7.00 MPa
@Strain 1.00 %
1020 psi
@Strain 1.00 %
ISO 604 (10)
 10.5 MPa
@Strain 2.00 %
1520 psi
@Strain 2.00 %
ISO 604 (10)
 17.0 MPa
@Strain 5.00 %
2470 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 10.7 J/cm²50.9 ft-lb/in²Partial Break; ISO 179-1/1eA
 12.8 J/cm²60.9 ft-lb/in²Double Notched
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+13 ohm1.00e+13 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 169 µm/m-°C94.0 µin/in-°FASTM E-831 (TMA)
 230 µm/m-°C
@Temperature 23.0 - 100 °C
128 µin/in-°F
@Temperature 73.4 - 212 °F
Melting Point 138 °C280 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 28.9 °C84.0 °FASTM D648
Minimum Service Temperature, Air -150 °C-238 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.