Ensinger PEI
Mitsubishi Chemical Advanced Materials Duratron™ D7015G PI Bearing Grade Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: This hot compression molded, 15% graphite filled PI is a bearing grade material with superior temperature and wear resistance, as well as a low coefficient of friction.

Available Properties
  • Specific Gravity
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Hardness, Shore D
  • Tensile Strength
  • Flexural Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Shear Strength
  • Charpy Impact, Notched
  • Surface Resistivity per Square
  • Dielectric Strength
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  • Data Sheet Region
  • Targeted Usage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.