Ensinger PEI
Mitsubishi Chemical Advanced Materials Duratron™ T4203 PAI Extruded Polyamide-imide
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Extruded

Material Notes: The ultimate PAI for impact strength and elongation, can bear high loads in extreme temperatures and offers exceptional dimensional stability and machinability.

Available Properties
  • Specific Gravity
  • Water Absorption at Saturation
  • Hardness, Rockwell E
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Yield
  • Flexural Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Shear Strength
  • Charpy Impact, Notched
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  • Data Sheet Region
  • Targeted Usage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.