Mitsubishi Chemical Advanced Materials Nylatron™ FST PA66 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Nylon shapes that are fire, smoke, and toxicity retardant, enabling them to withstand temperatures up to 347° F / 175° C. The first engineering plastic to achieve JAR / FAR 25.853 compliance, this polyimide grade was developed specifically for use in aircraft interior environments.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 88.088.0ASTM D785
Tensile Strength 90.0 MPa13100 psiISO 527-1/-2 (7)
Elongation at Yield 7.00 %7.00 %ISO 527-1/-2 (7)
Compressive Yield Strength  30.0 MPa
@Strain 1.00 %
4350 psi
@Strain 1.00 %
ISO 604 (10)
 60.0 MPa
@Strain 2.00 %
8700 psi
@Strain 2.00 %
ISO 604 (10)
 99.0 MPa
@Strain 5.00 %
14400 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.490 J/cm²2.33 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
 95.0 µm/m-°C
@Temperature 23.0 - 100 °C
52.8 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak LimitedLimited
Alcohols LimitedLimited
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.